[MW:1790] difference Between SA 542 and T/P24

Dear group,

can any body explain the difference between material SA 542 and T/P 24 

Though, both have all most same chemical composition but application is different. they are used in heavy thickness pressure vessel and boiler and steam tubing respectively. so plz let me know what is a difference between them metallurgically, and can we replace one by another among these two.?

chemical composotion is as 

Element

SA 542

T/P 24

C

0.14

0.05-0.10

Si

0.1

0.15-0.45

Mn

0.5

0.3-0.7

P

0.006

0.02Max

S

0.003

0.010Max

Cr

2.3

2.20-2.60

Mo

1.0

0.90-1.10

V

0.29

0.2-0.3

B

-

0.0015-0.0070































Regards,
Darshan Gambhava
9909910834


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...