[MW:1785] RE: 1783] Hydro test for vessels, heat exchangers and columns after 9 years of service in a petro chemical plant

Hi CSV,

 

Before proceeding with hydro test all thickness gauging and condition survey of vessel needs to be carried out, provided all are satisfactory and are meeting original vessel design thicknesses then vessels can be re-hydro tested at original test pressures, refer API 510 for more details.

 

Ravi

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Chandulal Vithlani
Sent: Thursday, March 19, 2009 12:06 PM
To: materials-welding@googlegroups.com
Subject: [MW:1783] Hydro test for vessels, heat exchangers and columns after 9 years of service in a petro chemical plant

 

I need help with respect to procedure to decide about the suitable hydro / pressure test pressure for the static equipments after service period of 9 years in a petrochemical plant. This should be with respect to the design pressure data available.

 

 

Regards

 

C S Vithlani

 

**********************************************************************

Borouge is a leading provider of value creating, innovative plastics solutions for customers in the Middle East, Asia-Pacific and Africa. Borouge employs unique Borstar® technology to produce differentiated products for high-value infrastructure applications, including water, gas and industrial pipe systems, power and communication cables, advanced packaging and automotive components. Borouge's state-of-the-art petrochemical complex is located at Ruwais, Abu Dhabi in the United Arab Emirates.

===================================================================================
CONFIDENTIALITY NOTICE

This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please delete the email and any attachment(s) and notify the sender.

This footnote also confirms that this email message has been scanned for the presence of computer viruses.
=============================================================================================================

 


 

~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
This email message is for the sole use of the intended recipient(s) and may contain confidential and privileged information of Cameron and its Operating Divisions. Any unauthorized use or disclosure is prohibited. If you are not the intended recipient, please contact the sender by reply email and delete and destroy all copies of the original message inclusive of any attachments.
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...