Hydrogen in steel is bad news for mechanical properties and the metal's chemical characteristics. A recent Key to Steel article details the chemistry of hydrogen problems. The feature also discusses the sources of hydrogen pick up in steel production from the addition of materials and components, such as lime and coke.
Wednesday, November 28, 2007
Minimize Hydrogen in Steel
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments: