Please refer to ASME sec IX - QW-200.2 & QW-401.1.
While ASME IX does not explicitly use the term "supplementary PQR", industry practice is to weld a new coupon
with the same WPS variables, which is issued as a new PQR; i.e., one cannot add hardness test results to the original
PQR, because that would not represent the same coupon. You must weld a new coupon and issue a new PQR with
hardness results, and cross-reference the original PQR if traceability is required.
C Sridhar.
is there any ref in code, pl share itTHANKS & BEST REGARDS,KG.PANDITHAN, BE, IWE, CSWIP 3.1,ISO 9712 Level 2 in VT,ASNT-Level II in PT,MT,RT & UT,LA ISO 9001-2015, ISO 3834, EN 15085,International Welding Engineer.CONSULTANT-WELDING & QUALITYMobile no: +919940739349--On Thu, Aug 28, 2025 at 6:20 PM sridhar cn <sridharcn305@gmail.com> wrote:You need to write in the new supplementary PQR format as the hardness testing date is current.Since the old PQR results (other than hardness values- as per the standard) are the same, it is not necessaryto enclose the old PQR. But, if your client insists, please act to satisfy him.C Sridhar.--On Thu, 28 Aug 2025 at 13:34, sridhar cn <sridharcn305@gmail.com> wrote:You can make a new, "Supplementary PQR" as it is safer and cleaner from a compliance and transparency
standpoint. You prepare a new PQR document with all the welding parameters repeated from the original PQR,
plus the new hardness test results.
You can add a note referencing the original PQR number (i.e., "This PQR was performed under the same welding
conditions as PQR-001 (provide actual details) to incorporate the hardness testing per client requirements").
C Sridhar.
On Thu, 28 Aug 2025 at 12:21, pankaj pachahara <pankajpachahara@gmail.com> wrote:Dear Experts,
We have a qualified PQR (P1 to P8) that doesn't include hardness testing. We're submitting this PQR for a new project, but the client requires hardness testing. To address this, we plan to:
1. Create a new PQR following the same parameters as the original PQR.
2. Conduct hardness testing and add the results to the new PQR.
We're unsure about the best approach to incorporate the hardness test results into our existing PQR documentation. We have two options:
Option 1- Add the hardness values to the original PQR as Addendum-1.
Option 2- Create a new PQR that includes all the previous data and name it as a Supplementary PQR.
Could you please guide us on the best approach to take?
Best regardsPankaj Choudhary--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJF_nWPufvGG-sFFjNLMxN8QYd3Dqo4DHA%2B8r_ocT1_7A2SbFA%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYih3EbLXznCG5Cb9-c6Sa%2B_z1T8fChrE1%2BZx9Z9rrJk-8Q%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM68D5VYocP2qb-NM7osefhAFbd_cENPpwTV7YfegCXgg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYihZqSvaVkL1GqKnWjmVQ%3Dt6XM6K769t70%2Bb6riFiVpTzQ%40mail.gmail.com.
Comments