[MW:32432] Allowable retubing in boiler as per IBR

Dear All,
Request to guide on how many times retubing is allowed in waste heat reboiler. We are currently doing it 3rd time in one of our reboiler.

Any IBR Code reference regarding this?

Regards
Devang Majithia

--