Dear sir,
Can I know the details of "ρ" in this equation ∆P= ρ.g.∆H
On Wed, Jul 26, 2017 at 11:12 PM, 'raouf salhi' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear chandra ,To calculate pressure difference between two points with difefrent level we have this formula :
∆P= ρ.g.∆HLe Mercredi 26 juillet 2017 14h15, Chandra Bhanu Mohapatra <bapunchandra@gmail.com> a écrit :
--Dear ExpertsAnybody kindly provide any guidelines or formulas for pressure loss calculation during hydrotest against the elevation (from 0 elevation to any height )--tHanks & rEgardsChandra Bhanu Mohapatra
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
Thanks & Regards.
SAKHILESHMON K S
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments