hi friends ,
               i am plan to do project in cold cracking .. as we all know cold crack occurs mainly due to diffusible hydrogen in weld metal and haz .. i want to determine the optimum level of  hydrogen  in haz  .. is there any method(test)  to determine the safe level of hydrogen .. in the haz

On Wed, Apr 23, 2008 at 8:09 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:


http://materials-welding.blogspot.com/2008/04/mw738-re-737-re-how-to-fin
d-hydrogen.html


Please check above link for the same.

-----Original Message-----
From: donboscomarine@vsnl.net [mailto:donboscomarine@vsnl.net]
Sent: Thursday, April 24, 2008 8:09 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:738] RE: 737] Re: how to find hydrogen concentration


Dear Mr. Bathula,

It is difficult to open a .DAT file. Will it be possible to send it as
any other attachment.

Thanks and best regards.

G. A. Soman
PRINCIPAL


----- Original Message -----
From: "Bathula Raghuram (Mumbai - PIPING)" <R.Bathula@ticb.com>
Date: Wednesday, April 23, 2008 9:23 pm
Subject: [MW:738] RE: 737] Re: how to find hydrogen concentration
To: materials-welding@googlegroups.com

>
> the formula is not appering in the message, hence resending as an
> attachment.
> -----Original Message-----
> From: materials-welding@googlegroups.com on behalf of Raghuram Bathula
> Sent: Wed 23/04/2008 20:51
> To: materials-welding@googlegroups.com
> Subject: [MW:737] Re: how to find hydrogen concentration
>
> May i know why you need this calculation? if possible please
> detaile it for
> the benifit of all members. probably the following would help you!
>
> This formula is used for detecting cracking susceptibility of
> steels and is
> valid only for certain range of steels
>
>
>
> Where *P*H is the cracking susceptibility parameter, H is the
> concentrationof hydrogen (in parts per million), *R*f is the
> restraint stress (in
> megapascals), and:
>
>
>
>
> Good luck!
>
> On Wed, Apr 23, 2008 at 3:28 PM, mech <arunmecheng@gmail.com> wrote:
> >
> > is there any mathematical formula to find  optimum level of hydrogen
> > concentration in steels
> >
> > >
> >
>
>
>
>
>
>
> >
>




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...