Hi everybody...
 
I have some problem in my design...
 
I was doing a Mechanical Dseign for a AES (TEMA type, single pass Heat Exchanger), where im supposed to design a Thin Wall Bellow on its Tube side.
 
The Design was  carried out for the Design pressure and it was satisfactory...
 
The Problem is.. i was askeed by the client to producee calculations for Hydro test condition and my design fails in that condition.. My question is DO I HAVE TO CONSIDER THE TEST PR During my design?
 
anyone please clarify...
 
Prabhakar.H 

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...