  Pig iron

 

  0.0000

  0.0999

  General-purpose grades for steelmaking

  0.1000

  0.1999

  General-purpose grades for casting

  0.2000

  0.2999

  Alloy pig iron

  Master alloys (deoxydants and alloying elements, including ferroalloys)

 

  0.3000

  0.3099

  Specular pig iron

  0.3100

  0.3199

  FeMn, Mn, FeSiMn

  0.3200

  0.3299

  Reserved

  0.3300

  0.3399

  FeSi, Si, FeSiZr

  0.3400

  0.3599

  Reserved

  0.3600

  0.3699

  FeAlSi,FeAlSiMn, NiSiMg, FeNiMg

  0.3700

  0.3799

  FeSiMg, NiMg,CaSiMg, NiSiMg, FeNiMg

  0.3800

  0.3899

  SiC, CaC2

  0.3900

  0.3999

  Reserved

  0.4000

  0.4099

  FeCr,FeCrSi,Cr

  0.4100

  0.4199

  Reserved

  0.4200

  0.4299

  FeMo

  0.4300

  0.4399

  FeW

  0.4400

  0.4499

  FeNi

  0.4500

  0.4599

  FeTi

  0.4600

  0.4699

  Reserved

  0.4700

  0.4799

  FeNb, FeV, FeTa

  0.4800

  0.4899

  FeB, FeP

  0.4900

  0.4999

  Reserved

  Cast iron types

 

  0.6000

  0.6999

  Grey cast iron

  0.6000

  0.6199

  unalloyed

  0.6200

  0.6299

  alloyed Cr

  0.6300

  0.6399

  alloyed Cu

  0.6400

  0.6499

  alloyed Mn

  0.6500

  0.6599

  alloyed Mo

  0.6600

  0.6699

  alloyed Ni

  0.6700

  0.6799

  alloyed Si

  0.6800

  0.6899

  others

  0.6900

  0.6999

  Reserved

  0.7000

  0.7999

  Ductile cast iron

  0.7000

  0.7199

  unalloyed

  0.7200

  0.7299

  alloyed Cr

  0.7300

  0.7399

  alloyed Cu

  0.7400

  0.7499

  alloyed Mn

  0.7500

  0.7599

  alloyed Mo

  0.7600

  0.7699

  alloyed Ni

  0.7700

  0.7799

  alloyed Si

  0.7800

  0.7899

  others

  0.7900

  0.7999

  Reserved

  0.8000

  0.8999

  Malleable cast iron

  0.8000

  0.8199

  unalloyed

  0.8200

  0.8299

  alloyed

  0.8300

  0.8999

  Reserved

  0.9000

  0.9999

  Special grades of cast iron

  0.9000

  0.9199

  unalloyed

  0.9200

  0.9299

  alloyed Cr

  0.9300

  0.9399

  alloyed Cu

  0.9400

  0.9499

  alloyed Mn

  0.9500

  0.9599

  alloyed Mo

  0.9600

  0.9699

  alloyed Ni

  0.9700

  0.9799

  alloyed Si

  0.9800

  0.9899

  others

  0.9900

  0.9999

  Reserved

  Reserved

 

  0.5000

  0.5999

  Reserved

 

 

 

 

  Non-alloy steels 

 

  1.0000 

  1.0099 

  Base steels 

  1.9000 

  1.9099 

  Base steels 

   

   

  Quality steels 

  1.0100 

  1.0199 

  General structural steels, with Rm < 500 MPa

  1.9100 

  1.9199 

  General structural steels, with Rm < 500 MPa

  1.0200 

  1.0299 

  Other structural steels not intended for heat treatment, with Rm < 500 MPa

  1.9200 

  1.9299 

  Other structural steels not intended for heat treatment, with Rm < 500 MPa

  1.0300 

  1.0399 

  Steels with average C < 0,12% or Rm < 400 MPa

  1.9300 

  1.9399 

  Steels with average C < 0,12% or Rm < 400 MPa

  1.0400 

  1.0499 

  Steels with average C >= 0,12% < 0,25% or Rm >= 500 MPa 

  1.9400 

  1.9499 

  Steels with average C >= 0,12% < 0,25% or Rm >= 500 MPa 

  1.0500 

  1.0599 

  Steels with average C >= 0,25% < 0,55% or Rm >= 500 < 700 MPa

  1.9500 

  1.9599 

  Steels with average C >= 0,25% < 0,55% or Rm >= 500 < 700 MPa

  1.0600 

  1.0699 

  Steels with average C >= 0,55% or Rm >= 700 MPa 

  1.9600 

  1.9699 

  Steels with average C >= 0,55% or Rm >= 700 MPa 

  1.0700 

  1.0799 

  Steels with higher P or S content 

  1.9700 

  1.9799 

  Steels with higher P or S content 

   

   

  Special steels 

  1.1000 

  1.1099 

  Steels with special physical properties 

  1.1100 

  1.1199 

  Structural pressure vessel and engeneering steels with C < 0,50%

  1.1200 

  1.1299 

  Structural pressure vessel and engeneering steels with C >= 0,50% 

  1.1300 

  1.1399 

  Structural pressure vessel and engeneering steels with special requirements 

  1.1400 

  1.1499 

  Special steels 

  1.1500 

  1.1899 

  Tool steels 

  1.1900 

  1.1999 

  Special steels 

  Alloy steels 

   

   

  Quality steels 

  1.0800 

  1.0899 

  Steels with special physical properties 

  1.9800 

  1.9899 

  Steels with special physical properties 

  1.0900 

  1.0999 

  Steels for other applications 

  1.9900 

  1.9999 

  Steels for other applications 

  1.2000 

  1.2999 

  Special steels - Tool steels 

  1.2000 

  1.2099 

  Cr 

  1.2100 

  1.2199 

  Cr-Si, Cr-Mn, Cr-Mn-Si 

  1.2200 

  1.2299 

  Cr-V, Cr-V-Si, Cr-V-Mn,Cr-V-Mn-Si 

  1.2300 

  1.2399 

  Cr-Mo, Cr-Mo-V, Mo-V 

  1.2400 

  1.2499 

  W, Cr-W 

  1.2500 

  1.2599 

  W-V, Cr-W-V 

  1.2600 

  1.2699 

  W, excluding groups 24,25 and 27 

  1.2700 

  1.2799 

  With Ni 

  1.2800 

  1.2899 

  Others 

  1.2900 

  1.2999 

  Special steels - Tool steels 

  1.3000 

  1.3999 

  Special steels - Miscellaneous steels 

  1.3000 

  1.3099 

  Special steels - Miscellaneous steels 

  1.3100 

  1.3199 

  Special steels - Miscellaneous steels 

  1.3200 

  1.3299 

  High speed steel with Co 

  1.3300 

  1.3399 

  High speed steel without Co 

  1.3400 

  1.3499 

  Special steels - Miscellaneous steels 

  1.3500 

  1.3599 

  Bearing steels 

  1.3600 

  1.3699 

  Materials with special magnetic properties, without Co 

  1.3700 

  1.3799 

  Materials with special magnetic properties, with Co 

  1.3800 

  1.3899 

  Materials with special physical properties, without Ni 

  1.3900 

  1.3999 

  Materials with special physical properties, with Ni 

  1.4000 

  1.4999 

  Special steels - Stainless and heat resisting steels 

  1.4000 

  1.4099 

  Stainless steel with < 2,5% Ni without Mo, Nb and Ti

  1.4100 

  1.4199 

  Stainless steel with < 2,5% Ni and Mo, but without Nb and Ti

  1.4200 

  1.4299 

  Special steels - Stainless and heat resisting steels 

  1.4300 

  1.4399 

  Stainless steel with => 2,5% Ni and Mo, but without Mo, Nb and Ti 

  1.4400 

  1.4499 

  Stainless steel with <= 2,5% Ni and Mo, but without Nb and Ti

  1.4500 

  1.4599 

  Stainless steel with special additions 

  1.4600 

  1.4699 

  Chemically resistant and high-temperature Ni alloys 

  1.4700 

  1.4799 

  Heat resistant steels with < 2,5% Ni

  1.4800 

  1.4899 

  Heat resistant steels with >= 2,5% Ni 

  1.4900 

  1.4999 

  Materials with elevated temperature properties 

  1.5000 

  1.8999 

  Special steels - Structural, pressure vessel and engineering steels 

  1.5000 

  1.5099 

  Mn, Si, Cu 

  1.5100 

  1.5199 

  Mn-Si, Mn-Cr 

  1.5200 

  1.5299 

  Mn-Cu, Mn-V, Si-V, Mn-Si-V 

  1.5300 

  1.5399 

  Mn-Ti, Si-Ti 

  1.5400 

  1.5499 

  Mo, Nb, Ti, V, W 

  1.5500 

  1.5599 

  B, Mn-B < 1,65% Mn

  1.5600 

  1.5699 

  Ni 

  1.5700 

  1.5799 

  Cr-Ni, with < 1,0% Cr

  1.5800 

  1.5899 

  Cr-Ni, with >= 1,0 < 1,5% Cr

  1.5900 

  1.5999 

  Cr-Ni, with >= 1,5 < 2,0% Cr

  1.6000 

  1.6099 

  Cr-Ni, with >= 2,0 < 3% Cr

  1.6100 

  1.6199 

  Special steels - Structural, pressure vessel and engineering steels 

  1.6200 

  1.6299 

  Ni-Sn, Ni-Mn, Ni-Cu 

  1.6300 

  1.6399 

  Ni-Mo, Ni-Mo-Mn, Ni-Mo-Cu, Ni-Mo-V, Ni-Mn-V 

  1.6400 

  1.6499 

  Special steels - Structural, pressure vessel and engineering steels 

  1.6500 

  1.6599 

  Cr-Ni-Mo, with < 0,4% Mo + < 2% Cr

  1.6600 

  1.6699 

  Cr-Ni-Mo, with < 0,4% Mo + >= 2,0 <3,5% Ni

  1.6700 

  1.6799 

  Cr-Ni-Mo, with < 0,4% Mo + >= 3,5 < 5,0% Ni oder >= 0,4% Mo 

  1.6800 

  1.6899 

  Cr-Ni-V, Cr-Ni-W, Cr-Ni-V-W 

  1.6900 

  1.6999 

  Cr-Ni except groups 57 bis 68 

  1.7000 

  1.7099 

  Cr, Cr-B 

  1.7100 

  1.7199 

  Cr-Si, Cr-Mn, Cr-Mn-B, Cr-Si-Mn 

  1.7200 

  1.7299 

  Cr-Mo, with < 0,35% Mo, Cr-Mo-B

  1.7300 

  1.7399 

  Cr-Mo with >= 0,35% Mo 

  1.7400 

  1.7499 

  Special steels - Structural, pressure vessel and engineering steels 

  1.7500 

  1.7599 

  Cr-V, with < 2,0% Cr

  1.7600 

  1.7699 

  Cr-V, with > 2,0% Cr 

  1.7700 

  1.7799 

  Cr-Mo-V 

  1.7800 

  1.7899 

  Special steels - Structural, pressure vessel and engineering steels 

  1.7900 

  1.7999 

  Cr-Mn-Mo, Cr-Mn-Mo-V 

  1.8000 

  1.8099 

  Cr-Si-Mo, Cr-Si-Mn-Mo, Cr-Si-Mo-V, Cr-Si-Mn-V 

  1.8100 

  1.8199 

  Cr-Si-V, Cr-Mn-V, Cr-Si-Mn-V 

  1.8200 

  1.8299 

  Cr-Mo-W, Cr-Mo-W-V 

  1.8300 

  1.8399 

  Special steels - Structural, pressure vessel and engineering steels 

  1.8400 

  1.8499 

  Cr-Si-Ti, Cr-Mn-Ti, Cr-Si-Mn-Ti 

  1.8500 

  1.8599 

  Nitriding steels 

  1.8600 

  1.8699 

  Special steels - Structural, pressure vessel and engineering steels 

  1.8700 

  1.8799 

  Steels not for heat treatment by user 

  1.8800 

  1.8999 

  Steels not for heat treatment by user (High strength weldable steels) 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...