[MW:33068] Transverse crack observed after fillet welding

Dear expert,

We observed transverse cracks after completion of fillet welding.
We are using EA2 filler wire in submerge arc welding and parent materials is E 450.
Please give us advice to resolve this issue.

Thanks & Regards

Kishore B 

No comments:

Re: [MW:35686] HDPE WPS