Austenitic steels are referred as non-heattreable in conventional sense i.e. they can’t be hardened by transformation hardening mechanism (quench & temper)

The only suitable method to increase strength/ hardness of austenitic grades is cold working.

 

In limited uses a surface treatment such as nitriding can also be tried but at the loss of corrosion resistance, however.

Following heat treatments apply to Austenitic grades:

Solution heat treatment

Stress relieving

Best Regards,

Iqbal 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sandy kumar
Sent: July 30, 2009 3:49 AM
To: materials-welding@googlegroups.com
Subject: [MW:2849] effect of heat treatment on Austentic Steel

 

Can anyone please tell about the effect of effect of heat treatment on Austentic Steel?

 

Regards

Sandeep kumar



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...