But the thickness should be upto 8 mm
Thanks & Best Regards
Saleem manhappulath
Mob:+966533595849
WhatsApp:+919526445936
From iPhone xs
Saleem manhappulath
Mob:+966533595849
WhatsApp:+919526445936
From iPhone xs
On Mon, 1 Sep 2025 at 1:59 PM guru <gurupadgs@gmail.com> wrote:
Dear team,Kindly clarify the problem which is as follows,I have CS wps gtaw+smaw (gtaw upto 8mm thk.)I have to weld 8"seh.40 (8.18mm)CS pipe with full TIG as per client requirement.Can I use the above WPS without SMAW (only GTAW upto 8 mm.thk)Thanks & Regards,--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2B-5weSNU4NhpPFUdSbYTzpH5c2vmOgaQxKpu2C-yW4Dn%2BnSdQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKH3Omuy0aJuk_jq22SPuceGG6KjZ_TyABseE%3DyC6Qrg53OiAQ%40mail.gmail.com.
Comments