Re: [MW:35631] HARDNESS TEST

Sir, 

Use Brinell or Rockwell C as per the heat treatment and material type.The test location, frequency, and acceptance criteria must comply with API 6A PSL level (usually PSL 2/3) and material class (AA, BB, CC...).

BR 
Deerendra

On Fri, 23 May, 2025, 18:12 Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Dear all
 
API6A FLANGE which hardness method recommended please guide me
Regard 
ELAVARASAN 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ykHf%3D_jc7zpJqgC1GYN4UkJ_aMLroy0YsnLNY2TO5oCNQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG0nF9GT77wWr0VUnaNkf4e8-oc%3D88j5Ahvp2mzjmasDofZSHg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...