Thursday, February 13, 2025

Re: [MW:35431] Welding Qualification for Shell with Rod full Penetration Welding

governing thickness is shell 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Feb 10, 2025 at 1:44 PM Shivasankar A <shivasankar2593@gmail.com> wrote:

Dear Friends,

Can you suggest me for a welding qualification for the above joint detail.

Material : Shell - SA 516 Gr.70
Rod : Duplex
Welding process: GTAW + SMAW

In my point of view, Plate to plate (Dissimilar) normal butt welding WPS & PQR is enough.  

Why I have a doubt is, here there is Diameter for Rod. So is there any Special Welding qualification for including the Diameter.

Please provide me the full step of Welding Qualification for the above Joint detail.


Regards,
A.Shivasankar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/c21ac9de-5d5f-4b97-91fd-882f63069a4bn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMRf2kuCjUspvAWaLz2SsBmqOCatL6C%2Bzwx8WHf7QeXPA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...