Thursday, November 7, 2024

[MW:35298] RF pad requirement

Dear Experts
I have a question regarding the RF pad design. If a vessel's RF pad is designed as a full RF pad but is facing fabrication issues such as the welding not being allowed to touch and potential concerns with bolt placement, how does that impact our calculations?
Specifically, if the cutting portion of the RF pad is affected, do we need to recalculate the entire design calculations for that RF pad?
Thanks in advance for your expert opinion.
Akash

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8af50cd0-aa0b-49b4-98aa-75904ea57197n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...