Re: [MW:35231] Re: Filler wire for 321H

ER347 is not meeting min C % requirement of 0.4%.
In that case, ER347 cannot be used. then which filler to be used?

On Friday, September 6, 2024 at 11:24:49 AM UTC+5:30 Mohd Siraj wrote:
ER 316H lacks the niobium stabilization that 321H requires for high-temperature applications 
and potentially leading to sensitization/reduced corrosion resistance in the heat-affected zone 

ER347 is the preferred filler material.  

On Friday, September 6, 2024 at 7:00:54 AM UTC+3 Mohmmed Dudhiyawala wrote:
Use ER316H.
We are successfully welding S321H, as per Russian GOST codes requirement.

On Wednesday, September 4, 2024 at 4:08:07 PM UTC+5:30 J Prinsen wrote:
Best use ER347H, Nb stabilized 18 10 Cr Ni steel

Regards

Jurgen Prinsen IWE


Van: "Kannayeram Gnanapandithan" <kgpan...@gmail.com>
Aan: "materials-welding" <material...@googlegroups.com>
Verzonden: Vrijdag 30 augustus 2024 10:21:33
Onderwerp: Re: [MW:35204] Re: Filler wire for 321H

ER 5356, is it not aluminium filler??

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Aug 30, 2024 at 1:36 PM trivikram kommala <trivikra...@gmail.com> wrote:
TIG 404 (ER 5356) - AWS / SFA 5.10



On Friday, August 23, 2024 at 8:07:57 AM UTC+5:30 Vignesh Manoharan wrote:
Hi experts, 

What filler wire is required to weld 321H in GTAW process. ? 

Pls suggest


Regards
Vignesh M

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a8e117c1-29b0-41aa-a8cf-c5ae26ab6c0an%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/01cf6c3a-931b-4635-86d6-a5189bc7d408n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...