Tuesday, September 10, 2024

Re: [MW:35218] Re: Filler wire for 321H

Best use ER347H, Nb stabilized 18 10 Cr Ni steel

Regards

Jurgen Prinsen IWE


Van: "Kannayeram Gnanapandithan" <kgpandithan@gmail.com>
Aan: "materials-welding" <materials-welding@googlegroups.com>
Verzonden: Vrijdag 30 augustus 2024 10:21:33
Onderwerp: Re: [MW:35204] Re: Filler wire for 321H

ER 5356, is it not aluminium filler??

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Aug 30, 2024 at 1:36 PM trivikram kommala <trivikramkommala@gmail.com> wrote:
TIG 404 (ER 5356) - AWS / SFA 5.10



On Friday, August 23, 2024 at 8:07:57 AM UTC+5:30 Vignesh Manoharan wrote:
Hi experts, 

What filler wire is required to weld 321H in GTAW process. ? 

Pls suggest


Regards
Vignesh M

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a8e117c1-29b0-41aa-a8cf-c5ae26ab6c0an%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOQkPcwNueayZFPJaEaAt%2BAzYS-ATMdPM%3DE1X%3DVajbw7g%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...