[MW:35206] Re: WELD DISTANCE AS PER API 650

refer api 650 section 7, its available.
before asking such straight question you could have refer code...
however there is no horizontal to horizontal value..only vertical offset..

On Thursday, August 29, 2024 at 12:36:10 PM UTC+3 Abd Ur Rehman wrote:
Daer expert what is the allowable distance between Vertical to Vertical & Horizantol to Horizantol Joints.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/48acfb39-6c8f-4571-af73-2fc70b6e0143n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...