Re: [MW:35151] Tolerances for Fillet weld Sizes as per ASME.


Hi Shivasankar,

I'm doing well, thank you! I hope you're doing well too.

For fillet weld size tolerance

AWS D1.1 Clause 5.24.3.2: Fillet welds can be up to 1/16 inch (1.6 mm) undersize, with no tolerance for oversize.

ASME B31.3 Paragraph 328.5.2: Fillet weld size should not be less than specified. There is no specified upper tolerance, but it should meet design requirements and construction code.

Refer to these sections in the latest editions of AWS D1.1 and ASME B31.3 for exact details.


Regards,
Dhatchanamoorthy.S

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"

On Thu, 1 Aug, 2024, 3:05 pm Shivasankar A, <shivasankar2593@gmail.com> wrote:
Hi Guys hope you all doing Good.


I need a clear idea about the Tolerances for Fillet Weld Size.

If my Fillet weld Size as per Drawing is 10mm. What will be the Tolerances.

Tell me the Exact location of this Tolerances given in the ASME.


Thanks in advance.

Regards,
A.Shivasankar 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/04774b1c-819d-48fd-95f8-7d21b3c6419dn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADNMk%2B%2BzBx1R9stVqUKGS0xZKuRjZMmKTX%3Dwnpo4zqJumyp0EQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...