Re: [MW:35090] Dear team,

Dear Ganesh, 
SUS304 (SUS meaning Steel Use Stainless) stainless steel austenite is typically known as the Japanese name for SS304 or AISI 304. The main difference between the two materials is not any physical property or feature, but how it is referenced in American and Japanese grades.

On Fri, Jun 28, 2024 at 5:17 PM Ganesh Rao <ga3677nesh@gmail.com> wrote:
Can please advice what is the meaning for SUS Material and what's are the heat treatment procedures. Attached details below.
Thanks in advance


From 
Ganesh  

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5bd7bc34-c172-422a-a7a2-28ad941e1566n%40googlegroups.com.


--
  
Anil Batawal
(Production Department) 
+91_9130053430
Pranit Chaudhari.
(Quality Control Engineer)
 +91_9359531288
LAXMI INDUSTRIES,
Gat No. 1539, Sonawane Wasti, Chikhali- Pune- 412114 
laxmi.ind11@gmail.comlaxmi.ind22@gmail.com .
khushal11.patil@gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJiH-%2BVZyVQ4z1nsEH1oZ_035b_pPdCpsHWnq-OB%3DCn5Wsh7qw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...