Friday, July 12, 2024

[MW:35110] Re: Information welding that presents crystallization

Explain the question with MOC & there welding.

On Thursday, July 4, 2024 at 8:45:36 AM UTC+5:30 Ildefonso Cabrera Reyes wrote:
Hello, can you give me some support on the prevention and care of welding that presents crystallization? 


Thanks.


Ildefonso Cabrera 
QC

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/42327d4b-95a6-40de-8df3-98eed6513d49n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...