[MW:35099] Re: PWHT Tripped !

3 joint in socking range- need re pwht.

other already in heating range so still temp not reach.

On Thursday, June 13, 2024 at 1:23:08 PM UTC+3 Parth Mandalaywala wrote:
I had 8 joint in PWHT process. 3 joints were Soaking stage while rest were in heating stage. Suddenly, the machine tripped. The technician was dumb & almost half hour passed by. My Concern is, do I start the whole process again or what? Pls, give answer with reference to code. I searched Sec 8, but found nothing. Any logical & practical solution will be appreciated.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/631c2300-219b-4c40-a481-4a5e656dc515n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...