Dear Saleem,

To determine whether you can use carbon steel (CS) material for welder qualification when you have a stainless steel (SS) Welding Procedure Specification (WPS) that is for P-8 to P-8 materials, we need to consider the relevant codes and standards governing welder qualification.

  1. WPS and P-Number Groups: The Welding Procedure Specification (WPS) you have is for welding P-8 to P-8 materials. In the ASME Boiler and Pressure Vessel Code (BPVC) Section IX, P-Numbers are used to group materials for welding qualification. P-8 refers to a group of austenitic stainless steels.

  2. Welder Performance Qualification: According to ASME Section IX, a welder's qualification is typically done to demonstrate their ability to produce sound welds. The welder qualification test should be performed using the same material group (P-Number) as the WPS. This ensures that the welder is proficient in welding the specific materials and processes described in the WPS.

  3. Using Different Materials for Qualification: ASME Section IX states that a welder qualified on a specific P-Number material is not automatically qualified to weld materials of a different P-Number. Therefore, if you use carbon steel (which is typically a P-1 material) for the welder qualification, this would not qualify the welder for welding P-8 materials (stainless steel) according to the WPS you have.

Summary:

No, you cannot use carbon steel (P-1 material) for welder qualification if your WPS is for stainless steel (P-8 to P-8). The welder must be qualified using materials that fall within the same P-Number grouping as specified in the WPS, which in this case is P-8 (austenitic stainless steel).

Recommendation:

To qualify a welder for the SS WPS (P-8 to P-8), you should use austenitic stainless steel materials for the qualification test to ensure compliance with ASME Section IX requirements.



On Tue, 7 May 2024 at 22:06, saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear All


    I have a ss wps P-8 to P8, i have plan to qualify welder. Can I use cs material for welder qualification with ss wps

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmvOBHxLj-_j4XRJQ-WwN6--u79GGcQr_zND%3DQE4ye%2B6QA%40mail.gmail.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAADcG1p7no00J%2BLvCPtPTw5HhenDUZ0JX0dfiRWiyBrJNgkvEg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...