Yes, you can use CS base material with SS filler and purging

On Tue, May 7, 2024 at 10:06 PM saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear All


    I have a ss wps P-8 to P8, i have plan to qualify welder. Can I use cs material for welder qualification with ss wps

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmvOBHxLj-_j4XRJQ-WwN6--u79GGcQr_zND%3DQE4ye%2B6QA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kE_3rwR%3Dztvxo8MsezHewrZN_CFbUh6WEsvSRcNXNjBg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...