Wednesday, May 29, 2024

Re: [MW:35033] welder qualification

Dear Saleem,

As per the AWS D1.1/D1.1M:2020 Structural Welding Code – Steel, the qualification range for a welder who qualifies on a 6" diameter pipe with a wall thickness of 10.97 mm using the specified electrodes (E6010 for root and hot pass, and E7018 for the fill and cap passes) would be as follows:

Diameter Qualification Range

  • When a welder qualifies on a pipe with a diameter of 6 inches, they are qualified to weld pipe diameters ranging from 2-7/8 inches (73 mm) and larger.

Thickness Qualification Range

  • If the test coupon has a thickness of 10.97 mm (approximately 7/16 inches), the welder would be qualified to weld material thicknesses ranging from 3/16 inches (5 mm) to 2 times the thickness of the test coupon. This results in a qualification range of 3/16 inches to 21.94 mm (approximately 7/8 inches).

Summary

  • Diameter Range: 2-7/8 inches (73 mm) and larger.
  • Thickness Range: 3/16 inches (5 mm) to 7/8 inches (21.94 mm).

These ranges are determined based on the requirements set forth in AWS D1.1, which provides the necessary guidelines to ensure welders are properly qualified for a range of diameters and thicknesses beyond their test coupon. It is important to note that these qualification ranges are contingent on the specific procedure and test details as outlined in the AWS D1.1 code. Always refer to the latest edition of the code for the most accurate and detailed information.


On Wed, 29 May 2024 at 10:14, saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear All

i am going to qualifying welder on pipe as per AWS D1.1

My question is if i qualify on 6" X 10.97, electrode e 6010 root+hot & e 7018 rest . whats is the qualification range for dia and thickness 



Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmtsQGJggFHLALaMyUJL%3DGzX2a3_zysrqKOz4n%2BvuFRs5A%40mail.gmail.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAADcG1pDE_Oxoi1ksNH5BV1G2MnxuBGQUv73quYx5A0y5NCyrA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...