Sunday, May 12, 2024

Re: [MW:34978] Welder qualification

Without backing qualified welder with backing also qualified.

On Wed, 8 May 2024, 9:12 pm Anup N K E, <nkeanup@gmail.com> wrote:
If welder is qualified using a CS WPS using TIG process (i.e. without backing and filler wire F-no. 6) then this welder is qualified to weld SS (i.e. with backing) with filler wire F no - 6.

Regards,

Anup NKE

On Wed, 8 May, 2024, 11:18 am kumar sumit, <kumarsumities@gmail.com> wrote:
I think, yes you can. Only TIG process. 

On Tue, 7 May, 2024, 7:35 pm saleem manhappulath, <saleemm9526@gmail.com> wrote:
Dear All


    I have a ss wps P-8 to P8, i have plan to qualify welder. Can I use cs material for welder qualification with ss wps

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmvOBHxLj-_j4XRJQ-WwN6--u79GGcQr_zND%3DQE4ye%2B6QA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACCHnjVhiyDvxN5dRw%3DENSCodzS%2BzaWLqNDSUkUkbF07goPQPQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJsQutZy6Pjswnse0BAQu0Afot3TumVCLDzwjBDSiij6R-4q2Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEabyKm5O%3D2a_ogFZ7QNOne1%3DSMXWF_NR7CTF4jG-3skG3a_ow%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...