Sunday, May 12, 2024

Re: [MW:34965] Impact value of Sa106 Gr B

Sa106 gr B not a impact tested material. It's not recommended for low temperature service. Refer ASME Sec VIII div1 UCS 66 for impact values.

On Tue, 7 May 2024, 5:26 pm Manish Kumar, <mkmkr431@gmail.com> wrote:
Hi,
Please share the impact value of carbon steel SA 106 Gr B.


Regards
Manish Kumar 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k6n2KTYcBFpAXdGOfh_4zF_a%3DggpuXXhecaP-Bmju0Tuw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEabyKkj1PjrFhFRa9URWNthWbcYOTBsFoo3nyKG0MnJ_WrPvA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...