Please ask some one in this group to send the MTC for dual certified grade of 316/316L as I do not have at this moment.

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Tuesday, 30 April, 2024 at 06:25:13 pm IST, Jenish Mistry <jenishmistry1992@gmail.com> wrote:


Dear sir ,

Can you share references/Documents  @ james Gerald ? 



On Mon, Apr 29, 2024 at 9:11 PM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
316 -   C:0.08max  UTS : min 75ksi
316L - C:0.03 max UTS : min 70ksi

For dual certified both the conditions to be satisfied.

Dual certified 316/316L   - C: 0.03 max  UTS : min 75ksi

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Monday, 29 April, 2024 at 08:05:51 pm IST, duybien.com <bck055@gmail.com> wrote:


Dual grade complied type 316 and 316L.
- Chemical composing of %C: < 0.03%, and
- Min. YS: 205 MPa.

Regards


On Thursday, April 25, 2024 at 4:35:46 PM UTC+7 kumar sumit wrote:
Dear expert, 
                      What is the meaning of dual grade lile 316/316L. Van anyone explain. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/9a3429f5-740c-4d61-8d6e-cb63f4782390n%40googlegroups.com
.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1961926607.2711332.1714402920064%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADXbd_e5NfYBhnNVsYKkc4wE%2BTz0%3DGGzzpXGqBMq48CTae_tqQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...