Re: [MW:34624] Regarding welding consumable for Material CuNi 90/10 (P34) to hastelloy C276(P43)

Check the UNS number of both material and refer ASME Sec.II C for equivalent UNS number range and filler material selection.

Chemical purity to be conformed on process base.


Regards

PRADEEP 

On Sat, 4 Nov, 2023, 16:07 Rahul ugale, <rahulugale23@gmail.com> wrote:
Dear All,
I have one query regarding welding compatibility of material combination -  CuNi 90/10  UNS C70600 (P34) TO  Hastelloy C276 material UNS NO: N10276 (P43)It is weldable ?
If it is weldable, then please suggest welding consumable.


Regards,

Rahul U.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c3594c6c-ab7c-4208-b913-596dbd1496a6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAWS%2BE8mM1M2kJb1zzGKdQJa1dJKCh1evboM7L3etJYPf2fXfg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...