[MW:34562] Re: Excess weaving in FCAW welding process

Dear Experts, 

The contractor is of the opinion that It is not an essential variable, hence it can be allowed. To substantiate their claim they say they will change the WPS and they will perform a hardness Test to prove that the properties were not changed. Please advise.

Best regards
Rajesh

On Sun, Oct 1, 2023 at 11:35 PM RAJESH KUMAR <rajeshkumarbhaskara@gmail.com> wrote:
Dear Experts,

Code:BSEN 15614-1:2017 ,BSEN 15609:2019 and DNV-OS-C401

I have noticed that WPS says the weaving is allowed/permitted 18 mm maximum for FCAW welding process.Please tell me whether we can allow if the weaving is more than the allowable limit.If it can be allowed.What is the reasons and on what basis it is allowed?If it can not/should not be allowed.Why and what is the reasons?


Thanks & Regards

Rajesh kumar
Dubai.



--



Thanks & Regards

Rajesh kumar
055-5251449
Sharjah

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMtcSfNED9XodhzawO%3Dv_2Q6Jx-VgA407eBg5d8uuK6fE%2BD6Zg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...