Sunday, September 24, 2023

Tube to Tubesheet mockup for HE and double pipe Exchangers.Re: [MW:34549] Tube to tube sheet WPS qualification

Dear All
Greetings for the day. 
We are carrying out a fabrication order which has
1) Double pipe Exchangers 
MOC CS to CS
Sizes 3" X 2" NB
 3" X 1" NB
2) Double pipe Exchangers 
MOC SS304 to SS304
Sizes 3" X 2" NB

3) Shell and PIPE Exchangers having Pipe to tubesheet joints
Moc Tubesheet 69mm thk SA387Gr. 11 to pipe 65NB Sch 80 SA335P11  . 

4) Shell and tube Exchangers having Tube SS304 to tubesheet SA387Gr. 11 joints
Moc CS to CS  sizes of tube :12.7OD  x 3thk 

5) Shell and tube Exchangers having Tube DSS31803 to tubesheet SA516Gr. 70 joints
  sizes of tube :12.7 OD x 3thk

My query is 
How many mock up test are to be established. 
Fabrication is as per SecVIII div 1.

Thanks in advance
Amit 9833859030

On Fri, 9 Sept, 2022, 10:25 am 'Prakash Hegde' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Hi
You req to qualify Mock up for T to Tsht joint as per secIX all reqmnt is addressed
This ll be used as PQR n  WPS also
Regards
Hegde


On Fri, 9 Sep 2022 at 10:09, sujit kumar
Dear sourav sir,

Thanks for the information whatever you have given it is really useful for me.......

sir I want to qualify new WPS for that tube-to-tube sheet because tube thickness is only 0.9 mm and tube od is 12.5 mm because I am not having WPS which lies in this thickness. please guide...??



On Fri, 9 Sept 2022 at 09:31, Sourav Bohrays <souravbohrays@gmail.com> wrote:
Dear sujit
If your code of construction is asme sec8 div1 no need of mockup you can use groove weld qualified wps for tuve to tubesheet
If code of construction is asme sec8 div2 its mandatory to do mockup.
If you have any earlier qualified tube to tubesheet mockup you can use by providing essential variable for tube to rubesheet in sec9



On Thu, 8 Sept 2022, 1:51 pm sujit kumar, <sujitkumar19942@gmail.com> wrote:
Hello sahil saini sir.

I would like to inform you that I know that clause but there is so many dought i am getting like 
If I want to do welding flange to tube....how to prepare WPS for that..???
Is there demonstration required for this tube to tube sheet...??

What test required in that WPS??

Please explain me it would be greatful  for me 

Best Regards
Sujit kumar


On Thu, Sep 8, 2022, 10:43 Shahil Saini <sainishahil98@gmail.com> wrote:
 Hello Sujit,

You shall refer ASME section IX Article-1 (QW-193) for tube to Tubesheet tests.

Thanks & Regards
Shahil Saini 

On Thu, Sep 8, 2022, 08:29 sujit kumar <sujitkumar19942@gmail.com> wrote:
Dear all,

Greeting for the day.

Please guide me regarding tube to tube sheet WPS Qualification.

We are having 8'' and 20'' flange and
 tube size 12mm Od 
thickness of the tube is 0.9 mm


Best regards
Sujit kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWMNorSJkBUKcBAS3_iwzbejVXnY0sSFL33yk4yxD7k46w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_8TFOFdwzb0VNs5v7HUkP7rGEAxgdG%2B8ktVovAgLxZKxA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWPkyV81QcDBOohZBnM_-ydBRAw7k1mjDm4Z6ZKEoYksDQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k_%3DfX15DzkcyNX4jXT6%2Bb2Zt3r%3D%3DZnt%3DEgUyg8bboV3SQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWMxScG2AD5Qw-tP1ivVYP4M%3DobbJwwF1g6YDgU%2BP9s3YA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1961491911.893313.1662699213698%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAABv9LD-xLJxA909cymJC6bd92-uZtpdoF5h2x5jdRzd%3DcryNg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...