Wednesday, July 12, 2023

Re: [MW:34403] ALLOY 825 IMPACT TEST REQUIREMENT AS PER ASME B31.3

First decide on the  Test temperature (MDMT). Test value will be based on Base material values.

Thanks & Regards

J.Gerald Jayakumar




On Wednesday, 12 July, 2023 at 01:20:40 pm IST, venkkates...@gmail.com <venkkateshkrishnan@gmail.com> wrote:


thank you, can you confirm the acceptance criteria of impact test value?

On Tuesday, June 20, 2023 at 11:49:33 AM UTC+3 james gerald wrote:
Yes if you use a different composition welding consumable compared to Base material

Thanks & Regards

J.Gerald Jayakumar




On Monday, 19 June, 2023 at 09:16:45 am IST, venkkates...@gmail.com <venkkates...@gmail.com> wrote:


Experts,

Please confirm that the weld metal impact test is required for solid alloy 825 pipe PQR using ENiCrMo-3 filler wire/electrode as per ASME B31.3 (Table 323.2.2 A-6).

Thanks in advance


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/954446a2-b8ee-47b7-984b-26fd84479d65n%40googlegroups.com
.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...