Re: [MW:34383] WPS FOR 321H

ER-347

On Wed, 5 Jul 2023, 22:48 Amit Udavant, <amitudavant@gmail.com> wrote:
ER 347.
Amit

On Wed, 5 Jul, 2023, 9:02 pm Ashish Chacko, <iamashleo007@gmail.com> wrote:
Dear experts , can anyone share me the wps for 321H.Am getting confused for the selection of filler material, ER347 or ER 16-8-2.Please support .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8a3d15da-5da8-456e-b984-e6477e5dc47en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAABv9LCoypsvUeDTEjcJOLx8nLHc7B%3D_F8OfUp3aQ9utPVL_2g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8nkcb4fDZkiSrtv8xZ%2BQXVAGhWdnuSSuAZJXSxocqVH3A%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...