[MW:34392] FILLER WIRE RECOMENDATION

Dear Experts ,

Kindly recommend filler wire and electrode for following metals:

1) A304H-A309
2)A304H-A321H
3)A321H-A321H

CONSIDER ALL OPERATION TEMPRATURE ABOVE 500 C.