Re: [MW:34347] PQR

 Thanks I see QW 211 ASME IX that explain for the material 

Sent from my iPhone

On Jun 19, 2023, at 12:16, Keribo Berepele <berepele@gmail.com> wrote:


please can i site it in any where, document please

On Mon, Jun 19, 2023 at 11:55 AM Ritesh Kumar Singh <riteshsiwan770@gmail.com> wrote:
Yes You can  position is non essential variable in WPS.

On Mon, 19 Jun 2023, 4:00 PM Keribo Berepele <berepele@gmail.com> wrote:
Dear Experts, please confirm if plate 3G welding can be used to perform PQR for a 6G 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF27W4SF2pzp_dB4Qp0aBKsm%3D82odEd8DGReLJ4eEK_iEf8CZw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-jw2s8%2B3zprob6YSY8xQ%3Dnhb8gR0bO67pAJDO7hgiazHw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...