In my opinion you can not weld 25 mm thk.

On Sunday, June 18, 2023 at 9:40:34 AM UTC+5:30 sujit kumar wrote:
Dear all,

I am having material thickness SS316   25 mm to weld.
1.  i have qualified  GTAW PROCESS WPS with  10mm plate which is allow 2T up to 20 mm  thk weld 
2. another i have qualified SMAW with back chip WPS with 10 mm Plate which is allow up to  20 mm SMAW only with Back chip.

may i allow to do 25 mm thick welding with Both  gtaw +smaw  welding.




sujit

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a3a44be3-3213-472d-a988-74d9ca8917acn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...