[MW:34310] Re: Gas purity conformation

You can use 99.5 % 
Pl. qualify PQR and address in WPS as
Shielding Gas - CO2 
Composition - 99.5 % minimum 

In the said case you can NOT write Shielding gas - SFA 5.32  SG-C in WPS ,PQR 

Thanks and regards

Vishwas -IWE 

On Monday, June 12, 2023 at 4:16:06 PM UTC+5:30 JITHIN GOPINATH wrote:
Sir,
 As per sec IX and API 1104 purity of gas is not an essential variable but in sec II C they had mentioned about the purity percentage. For example I have a gas certificate for CO2 with 99.5% but as per sec II C the purity percentage is given as 99.8%.
 So please advise me can I go with 99.5%...


Thanks and Regards

Jithin 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/92072d7f-fb49-49d5-ad75-ea770b34d758n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...