Re: [MW:34239] ER80S-G/ER80S-Ni1

What is the composition of 
ER80S-G
ER80S-Ni1

Send   MTCs  of both  the consumables

On Tue, May 23, 2023 at 1:20 PM Baqer Shabbeer <engbaqer@gmail.com> wrote:

Dear experts,

I would appreciate your valuable response regarding the following inquiry.

The filler wire mentioned below is approved for our normal Gas Metal Arc Welding (GMAW) Welding Procedure Specification (WPS):

·        AWS Classification: ER80S-G

·        SFA Specification: 5.28

·        API 1104 Group: 5

·        Trade Name: PIPELINER 80Ni1

·        Base metal API 5L Gr. X65

However, for repair welding joints, our approved WPS (GMAW Welding) specifies the use of the following filler wire:

·        AWS Classification: ER80S-Ni1

·        SFA Specification: 5.28

·        API 1104 Group: 5

·        Trade Name: PIPELINER 80Ni1

·        Base metal API 5L Gr. X65

Unfortunately, my team used AWS Classification ER80S-G for the repair welding using Repair WPS.

I would like to know if this deviation is acceptable or if any corrective actions are necessary.

Thank you for your expertise and guidance.


Regards,

Baqer


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/30a48598-af6d-4f67-9b81-dcd6e1d9f3a1n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3OFzmNAi8btPaUzrmXcLhRrjmaT_v5%2BzFLTnv6wCeaRZA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...