Tuesday, May 16, 2023

RE: [MW:34207] RE: 34198] tubular bevel problem in TYK joint in AWS D1.1

Please see the below:

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Duong Vinh Quang
Sent: Tuesday, May 9, 2023 10:42 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:34204] RE: 34198] tubular bevel problem in TYK joint in AWS D1.1

 

In aws d1.1, no show about bevel angle, pls check and hep me

 

On Mon, May 8, 2023, 8:19 PM <xuanthong.hp@gmail.com> wrote:

Hi sir,

Pls see the clause 10/ AWS D1.1,

You can see the detail at Figure 10.5 to 10.10

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Duong Vinh Quang
Sent: Saturday, May 6, 2023 10:28 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:34198] tubular bevel problem in TYK joint in AWS D1.1

 

Hi everyone, I would like to ask about the beveling issue in the AWS D1.1 standard when welding tubular in TYK joint, what part of the beveling issue is covered in AWD D1.1. I can not find it.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b0f27ff7-32e2-49b4-a97c-ded6879eb9d9n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/70bd01d98101%2454731980%24fd594c80%24%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOdNLKgSSp%2B-uKkhDiEjUkVA-iv%2Be0CujFrjeGjO_VHkuzyTPw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...