Re: [MW:34031] Percentage of Consumables for Steel Structure

Theoretically, it is 2 to 3% of the weight of the material used in sheet metal fabrication.
For thick plate materials, it is  3 to 4%.  In practice, it can go up by another 2% or so due to 
unwanted and extra reinforcement and large fillet sizes.
Sridhar.

 

 Friday, 24 February, 2023 at 03:23:57 pm IST, Saleem Khan <mail.salemkhan@gmail.com> wrote:


Hi Experts,

Hope that you are all fine and doing great. 

I need to Estimate Percentage of Consumables in Steel Structure, I know the details of  calculation but need to develop rule of thumb. 

will you please share your experience with me.

Regards,

Saleem Khan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8a157d08-1ffb-4171-8cf4-c921a06a5dc3n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...