Tuesday, February 7, 2023

Re: [MW:34004] Hardness Test on Stainless Steel and Carbon Steel

Is it for production Harness testing or weldimg PQR or parent base metal Hardness testing

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, 7 February, 2023 at 08:28:25 am IST, furkan topaloğlu <topaloglufurkan8@gmail.com> wrote:


Dear Experts,

I would like to ask a question regarding the hardness test on Stainless Steel and Carbon Steel.

Do I need a different calibration block for SS / CS or another probe for these different types of material?

Can I use the same probe on the SS and CS material without additional calibration ?

Could you please inform me with technical background ?

Thanks in advance. Regards

--

Regards / Saygılarımla

 

Furkan TOPALOĞLU

Metallurgy and Material & Welding Engineer

Phone : +7 916 524 21 02

              +90 539 437 88 03

E-Mail : topaloglufurkan8@gmail.com

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALZR%3D4Q7gznnLQyDu9jE%2BaGYekvWSr5aLxMdP%3DYSSBYTitCk9g%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...