11.4 hrs total.

2.7 hr for rate of heating and 6 hrs holding time and 2.7 hrs for rate of cooling so in total : 11.4hrs

On Sat, Oct 8, 2022 at 2:15 PM Student <nabeel233@gmail.com> wrote:
The following is an exam question. Please guide how to do it

A  one and Half inch of material has to be PWHTed from 600 F to 1350  and shall be kept at 1350 F for 6 hours. It has to be cooled down back to 600 F. If the rate of heating and cooling is 500F per hour per inch  , what is the total time for PWHT.  Do not consider heating the material up to 600F in the calculation

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/472dc2c2-2914-4cb4-abf5-a400e882886fn%40googlegroups.com.


--
Thanks and Regards
Aravind Vadrapalli
QA (Certified Senior Multi Discipline Inspector)
Email address: aravind.mec@ gmail.com
Contact No : +917675039689

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2ByoLnDaobZmY%2BCqMnh9FC0Yz_3cq5O4Tp6uBczngLL2xOvWVg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...