That's correct since the welding technique to weld Inconel is entirely different than normal steel/CS.



On Monday, January 30, 2023 at 11:31:38 AM UTC+3 Szymon Ossowski wrote:
Hi, 

I have made Welder Performance qualification with using P-no. 8 and F-no. 6.

Asme IX gives for welder qualification for: P-no. 1-15F; P-no. 34, and P-no. 41-49
Than he can weld Inconel Base metals

But F-no 6 gives for welder qualification for use only all F-no. 6. 
F-no. 6 don't give for him permission for welding inconel filler materials 

Am I correct?

What for the welder is given permission in welding Inconel materials but not with F-no 41-46???

Do someone can help with this misunderstanding?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/368a36bc-9a25-483d-8a92-4533e1c97c35n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...