Friday, January 6, 2023

RE: [MW:33900] Re: ASTM A53 Gr.B TYPE E equivalent in ASTM

EN 10217-1 does not contain S275JR. S275JR is a structural steel acc to EN 10025-2. It covers plates and open sections – not pipes.

Structural pipes is found in EN 10210 and EN 10219.

 

EN 10217-1 is for pipes for pressure purposes and have type P195, P235 and P265.

 

Kind regards

Kristian Lund Jepsen

Senior Chief Consultant

 

D +45 51617324

M +45 51617324

kuj@ramboll.com

Rambøll Danmark A/S, DK REG. NO. 35128417
Registered office: Hannemanns Allé 53, 2300 Copenhagen S

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Kannayeram Gnanapandithan
Sent: 5. januar 2023 10:48
To: materials-welding@googlegroups.com
Subject: Re: [MW:33895] Re: ASTM A53 Gr.B TYPE E equivalent in ASTM

 

ASTM A 53 is a Pipe material specification


THANKS & BEST REGARDS,

KG.PANDITHAN, BE, IWE,  CSWIP 3.1,

ISO 9712 Level 2 in VT,

ASNT-Level II in PT,MT,RT & UT,

LA ISO 9001-2015,

International Welding Engineer. 

CONSULTANT-WELDING & QUALITY

Mobile no: +919940739349

 

 

On Thu, Jan 5, 2023 at 12:04 PM Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:

Pl. prepare comparative statement in detail  for both the Materials of interest.

Consult Engineer - Design

Jointly discuss the service application of the component under fabrication for which you are intending to change the MOC and then decide the material selection .

 

Regards

 

Vishwas -IWE 

International Welding Engineer

 

On Thursday, January 5, 2023 at 9:33:30 AM UTC+5:30 Sami MERT wrote:

Dear All,

 

Is ASTM A53 Gr.B TYPE E equivalent properties with S275JR (EN 10217-1) ? Could we use it instead of ASTM A53 Gr.B TYPE E?

 

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b9c7a47d-885a-4e6a-bbc4-6f11afa99ad7n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNmySJbxQGxaauDfHGoyc2xRqVnhC3-t9giD7dMVT%3Dwbg%40mail.gmail.com.


Classification: Confidential

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...