For welding barrier layer of Clad steel it is recommended to use 65% Nickel-copper(Monel) filler Rod / Electrodes & remaining overlay may be welded using 70-30 Cu-Ni or 90-10 CuNi electrodes accoring to the requirements. 

Please see snap shot below.

Inline image


Inline image



Thanks & Regards

J.Gerald Jayakumar




On Monday, 2 January, 2023 at 03:41:37 pm IST, mohit aggarwal <aggarwalmoh@gmail.com> wrote:


Hello Experts,

I have query regarding use of Cu Ni 90/10 consumable for overlay  with support of Cu Ni 70/30 weld overlay procedure  qualification or I will have to qualify new procedure with use of CU/Ni 90/10 consumable.

Regards,
Mohit.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3520c98c-291d-482d-8fd2-d91abf2d79f3n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...