[MW:33955] Unequal wall thickness same base metel

Dears, 
    Clarify same base metal but different  wall thickness(11.97 and 7.9mm)please any tolerance for fitup and standard.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHt4qw8iA06jXxB4BtkBuT9oXtSAZ4%2B7E7zt0vsV6m7U%2Bj0XUw%40mail.gmail.com.