Friday, December 23, 2022

Re: [MW:33851] Single pass fillet weld (6 mm leg length) using 1mm GMAW wire

Please read it as " There are no code limitations" 
By oversight, the word no was omitted. Regret the error.
sridhar.
--------------------------------------------------------------------------


On Thursday, 22 December, 2022 at 09:19:40 am IST, 'Sridhar Cn' via Materials & Welding <materials-welding@googlegroups.com> wrote:


There are code limitations in achieving fillet sizes. You can get even a
8 mm size fillet using 1.00 mm filler wire in a single pass or a 6 mm 
fillet using 0.80 mm size wire also.
Select your parameters to achieve the required fusion and penetration
without an undercut.

Sridhar.
-------------------------------------------------------------------------------------------

On Tuesday, 20 December, 2022 at 08:49:28 am IST, Ganesh R nair <ganeshrnair9@gmail.com> wrote:


Dear all,

Is there any code limitations to use 1mm mig wire to achieve 6mm fillet weld (leg length) in a single pass.

Thanks,
Ganesh R Nair

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ_8oJX7W1BVjNm%2Bh%2B%2BFJkD9K9Tky1Xtuop%2B2EhZmxHHCYriwQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1313242092.2100972.1671679235531%40mail.yahoo.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...