Monday, December 19, 2022

Re: [MW:33832] Re: Vanadium composition showing in p91

0.004 % V- its trace element  
Not a deliberate addition


On Monday, December 19, 2022 at 8:54:33 AM UTC+5:30 mithlesh kumar wrote:
Vandium % is .004

On Mon, Dec 19, 2022, 8:43 AM Vishwas Keskar Welding Manager WELDING <vvkes...@gmail.com> wrote:
What is the % Vanadium in that MTC ?
It is trace elements not a deliberate addition for Gr 22  unlike Gr 91 where it it MUST in Gr 91 

Regards

Vishwas IWE
International Welding Engineer 


On Saturday, December 17, 2022 at 8:47:13 PM UTC+5:30 mithlesh kumar wrote:
Kindly read WP22 instead of P91
On Saturday, December 17, 2022 at 8:15:23 PM UTC+5:30 mithlesh kumar wrote:
Dear team,

I have observed vanadium in heat analysis of p91 MTC  , but as per code vanadium is not showing in chemical composition table. Suggest is it acceptable or not if acceptable code reference please.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/UmVRYgreKIE/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1f2331d9-3cb1-437c-adc3-ba7b8be6f9f8n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c9a869db-a1c1-4267-a60a-aa786edd4e03n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...