Wednesday, November 30, 2022

Re: [MW:33790] Filler wire Button weld test

Dear 
See how you will ensure at the receiving stage you received the correct alloy material(Consumables) tell me ????
The weld button is like a test coupon where the PMI probe can easily seat and you can verify the chemistry.

I am working on ARAMCO specs, for us it's mandatory requirement

due to PMI prob inaccessibility on material like consumables and weld , weld button is alternate, in Aramco Spec

check ASME /ASTM for PMI requirements.



Faisal. Q

Sr.Mechanical Inspector,

 

ENERGY & INDUSTRY DIVISION

Dhahran, 34247-2958

Kingdom of Saudi Arabia.

M: +966 537134558

E: faisal.quadri@applusvelosi.com

 


 

 



On Tue, Nov 29, 2022 at 1:25 PM Ponnikumar <k.ponni1994@gmail.com> wrote:
Dear gentlemen,
My client inspector told me to do button weld test on plate for filler wire 309L . The dimension are follow as asme sec II c then need to do PMI verification 

My query is any requirements by code for filler wire button test for all filler and electrode and why it required ? 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKL%3DdYw73OyFYLq4yTHUB2cVqbuaDCCunxc73%2BaU0kJZurJd%2Bw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJwxg4fPH7WMGoY70x98jSpb%3DHWH7X1QY%2BdCzoCW5ZNSDRkQaA%40mail.gmail.com.