Thursday, November 24, 2022

Re: [MW:33764]

SMAW with E 7018 electrode Or  CO2 Welding.

On Tue, 22 Nov 2022, 13:44 ahmed adil, <ahmed.adil5382@gmail.com> wrote:
Dear Vishal

Oxyacetylene welding or Thermit welding are suitable for your job

Best wishes
Ahmed Adil
Welding engineer 

On Mon, 21 Nov 2022, 06:48 Vishal Jaiswal, <vis469jaiswal70@gmail.com> wrote:
Dear All, 

Please suggest wihich welding is sutaible for GI flat bar to GI flat bar  used in cable tray and also which WPS is use for 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF6t40-BfGWU15koamWdVZ4NsvN_v7mgs69dDW0V6BE%2BUSHqDA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPZgYYx55KmdEzhaTv5xYSxHGF0zirQia1FXbuFowy%3DSRmpS-g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGhQL0mRn9-_mvgd6Mzbjpy-pRorWDz7LeZEtqRwBa49%3Dw7ycA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...